Por favor, use este identificador para citar o enlazar este ítem:
http://dspace.espoch.edu.ec/handle/123456789/5231
Registro completo de metadatos
Campo DC | Valor | Lengua/Idioma |
---|---|---|
dc.contributor.advisor | Sánchez Herrera, Tatiana Elizabeth | - |
dc.contributor.author | Romero Guanotasig, Danilo Fernando | - |
dc.date.accessioned | 2016-10-13T15:44:46Z | - |
dc.date.available | 2016-10-13T15:44:46Z | - |
dc.date.issued | 2015-12 | - |
dc.identifier.citation | Romero Guanotasig, Danilo Fernando. (2015). Obtención de cuero gamulán con la utilización de diferentes niveles de formaldehido en conbinación con sulfato de aluminio. Escuela Superior Politécnica de Chimborazo. Riobamba. | es_ES |
dc.identifier.uri | http://dspace.espoch.edu.ec/handle/123456789/5231 | - |
dc.description | .En las instalaciones del Laboratorio de Curtiembre de pieles de la FCP de la ESPOCH, se evaluó el efecto de tres niveles de formaldehido (4, 5, 6 %), más el 4% de sulfato de aluminio, en la curtición de 24 pieles ovinas para la producción de cuero gamulan, divididas en 3 tratamientos y 8 repeticiones, modeladas con un DCA simple, llegando a determinarse con el 6% de formaldehido el mejor porcentaje de elongación (54,69%), y resistencia a la tensión (1431,83 N/cm2), la mejor naturalidad (4,88 puntos); blandura ( 4,75 puntos) y tacto ( 4,63 puntos); es decir, el producto que se logró presenta una belleza visual, suavidad, caída y tacto agradable. El cuero gamulan es un producto muy difícil para la confección; puesto que, se debe cuidar que la lana no sufra debilitamiento del bulbo piloso de tal manera no se desprenda fácilmente al confeccionar o al utilizar el artículo. La evaluación económica determinó respuestas favorables al aplicar 6% de formaldehido ya que la relación beneficio costo fue de 1,30, o una ganancia del 30% que supera ampliamente con las de otras actividades similares pero con el beneficio de que la recuperación del capital es más rápida y su margen de riesgo es menor al de otras producciones. Por lo que se recomienda utilizar 6% de formaldehido para obtener cueros con buenas resistencias físicas y calificaciones sensoriales, indispensables para que los artículos confeccionados sean resistentes y sobre todo conserven tanto la belleza natural en el cuero como en la lana. | es_ES |
dc.description.abstract | This research was carried out in the leather tannery lab of Livestock Science Faculty of ESPOCH, in order to determine the effect of formaldehyde (4, 5, 6 %) plus 4 % of aluminum sulfate to produce gamulán leather. It was tested to tan 24 sheepskin, the test consisted of 3 treatments and 8 repetitions modeled with DCA simple, which revealed that the treatment with a 6 % of formaldehyde is the best since it gave the best results in regarding elongation percentage equal to 58,13 % and the resistance to the tension equal to (1431,83 N/cm2); the natural consistency equal to (4,88 points); and the smoothness equal to (4,75% points); and touch equal to (4,63 points); therefore the target product kept visual beauty, a pleasant smoothness, falling, and texture. The gamulán leather from sheepskin is very difficult to be produced since the wool hairy bulb damage must be prevented in order to the wool were not easily detached at the very moment of prepare and make the final product. The economic assessment were carried out in regarding cost-benefit which determined that the treatment with a 6% of formaldehyde gives a 30% of profitability which represents a rate of return of 1,30 and which widely overcomes the profitability from other activities since the capital return faster and the margin of error is smaller than the other similar activities since the capital return is faster an margin of error is smaller than the other activities. Therefore is advisable to use the 6% formaldehyde to make the best sheepskin leather not only for the physical resistance but also for the sensorial quality features which is essential for the products made of gamulán leather were resistant and the well as wool natural beauty were well conserved | es_ES |
dc.language.iso | spa | es_ES |
dc.publisher | Escuela Superior Politécnica de Chimborazo | es_ES |
dc.relation.ispartofseries | UDCTFCP;17T1316 | - |
dc.rights | info:eu-repo/semantics/openAccess | es_ES |
dc.subject | CUERO GUAMULÁN | es_ES |
dc.subject | FORMALDEHIDO | es_ES |
dc.subject | SULFATO DE ALUMINIO | es_ES |
dc.subject | RIOBAMBA (CANTÓN) | es_ES |
dc.subject | CHIMBORAZO (PROVINCIA) | es_ES |
dc.title | Obtención de cuero gamulán con la utilización de diferentes niveles de formaldehido en conbinación con sulfato de aluminio | es_ES |
dc.type | bachelorThesis | es_ES |
dc.contributor.miembrotribunal | Hidalgo Almeida, Luis Eduardo | - |
dc.rights.uri | https://creativecommons.org/licenses/by-nc-sa/3.0/ec/ | es_ES |
Aparece en las colecciones: | Ingeniero/a Zootécnista |
Ficheros en este ítem:
Fichero | Descripción | Tamaño | Formato | |
---|---|---|---|---|
tesis completa danilo.pdf | 1,25 MB | Adobe PDF | Visualizar/Abrir |
Este ítem está sujeto a una licencia Creative Commons Licencia Creative Commons